2012-05-29 23:00:55

Quench-Kleen 5343 from Houghton International is a low-residue alkaline spray cleaner specifically formulated for heat-treating applications. Valley Forge, PA

2011-10-21 13:00:00

Wisconsin Oven designed and manufactured a gas-fired heavy during box furnace to anneal spools of aluminum wire used in electrical cables.

2008-10-02 03:00:33

By Soliman, Mohamed Palkowski, Heinz Two Mo-Nb microalloyed transformation-induced-plasticity (TRIP) steels, with Al contents of 0.23 and 0.65, were subjected to several hot-rolling conditions designed to generate different ferrite morphologies and grain sizes.

2008-09-05 03:00:22

By Timelli, Giulio Lohne, Otto; Arnberg, Lars; Laukli, Hans Ivar The influence of solution heat treatment time and temperature on the microstructure and mechanical properties and the mode of fracture of a high-pressure die-cast AlSi7MgMn alloy is reported.

2008-08-22 09:00:53

Regulatory News: To meet increasingly strong global demand for quenched and tempered (Q&T) steels, SSAB today announced a SEK 5.3 billion investment program to further develop the company's production base in Sweden and the United States.

2008-07-26 03:00:29

By Mintz, B Gunawardana, W D; Su, H Aluminium in solution in the ferrite in ferrite/pearlite steels has been found to have little influence on strength of the ferrite probably because up-till recently it has been added in very small amounts (0.02-0.08 wt-%Al) as a grain refining addition.

2008-02-29 03:00:30

By Trabadelo, V Iturriza, I The microstructure of powder metallurgy T42 high speed steel has been analysed after isothermal annealing.

2008-02-29 03:00:27

By Das, S Singh, S B; Mohanty, O N; Bhadeshia, H K D H The basic science behind bake hardening steels is well understood in terms of the interactions between interstitial solutes and dislocations.

2006-11-01 06:01:59

By Villanueva, D M E; Junior, F C P; Plaut, R L; Padilha, A F The present work studies, in a comparative manner, the sigma phase precipitation of three stainless steels: austenitic type 316L (17Cr-12Ni-2.5Mo, wt-%), superferritic type DIN W. Nr. 1.4575 (Nb- 28Cr-4Ni-2Mo, wt-%) and duplex type DIN W.